Ukonakala okanye ukujika kombalaucingo lwentsimbikwiatmosfera ebangelwa yioksijini, ukufuma kunye nobunye ukungcola okungcolisekileyo kubizwa ngokuba ngumhlwa okanye umhlwa.Emva kokuvuswa kocingo lwentsimbi, kuya kuchaphazela umgangatho wenkangeleko, kuchaphazela ngokunzulu ukusetyenziswa, kwaye kubangele i-scrap, ngoko ucingo lwentsimbi kufuneka lugcinwe ngokufanelekileyo kwaye lunikele ingqalelo kuthintelo lomhlwa.
Zinc adhesion onucingo lwezinkiumphezulu kunye nobukhulu be-zinc layer
A. Xa ubukhulu be-plating bu-3-4 mm, i-zinc adhesion kufuneka ibe ngaphantsi kwe-460g / m, oko kukuthi, ubukhulu obuqhelekileyo be-zinc layer ayikho ngaphantsi kwe-65 microns.
B. Xa ubukhulu be-plating bukhulu kune-4 mm, i-zinc adhesion akufanele ibe ngaphantsi kwe-610g / m, oko kukuthi, ubukhulu obuqhelekileyo be-zinc layer akufanele bube ngaphantsi kwe-86 microns.
C, ukufana kokugquma: umaleko wegalvanized ngokusisiseko ufana novavanyo lwesisombululo sobhedu sesulfate efakwe kahlanu ngaphandle kokuveza intsimbi.
D, ukuncamathelisa ukutyabeka;I-zinc layer ye-plating parts kufuneka idibaniswe ngokuqinileyo kunye nesiseko sesinyithi esinamandla okwaneleyo okubambelela, kwaye ayiyi kuwa okanye iqhube emva kovavanyo lwesando.